Creep Properties of Heat Resistant Steels and Superalloys, 2004th Edition

Advanced Materials and Technologies

$5,841.32
  • Hybrid

    365 pages

  • Release Date

    24 May 2004

Check Delivery Options

Summary

For environmental reasons it is necessary to increase the process temperature in power plants and in industry, e.g. in chemical plants. This implies the development of steels and alloys that can be used at high temperatures and severe conditions. These materials need to be capable of enduring long-term use. On the other hand, equipment and plants built in the 1970s have become aged and their control requires a high degree of accuracy to ensure their safe operation. In this case, the most important property of the materials is creep, especially long-term creep, and thus it is necessary to evaluate and estimate long-term creep strength more accurately. It is therefore a top priority to accumulate data and knowledge about creep and to share the information.

This volume contains a compilation of long-term creep and rupture data and knowledge based on these data on heat resistant steels and superalloys, collected by three leading creep research organizations and agencies, namely: ECCC (European Creep Collaborative Committee), GCC (German Creep Committee) and NIMS (National Institute for Materials Science) of Japan.

Book Details

ISBN-13:9783540428794
ISBN-10:3540428798
Author:K. Yagi, G. Merckling, T.U. Kern, H. Irie, H. Warlimont
Publisher:Springer-Verlag Berlin and Heidelberg GmbH & Co. KG
Imprint:Springer-Verlag Berlin and Heidelberg GmbH & Co. K
Format:Hybrid
Number of Pages:365
Edition:2004th
Release Date:24 May 2004
Weight:1.26kg
Dimensions:193mm x 270mm
Series:Landolt-Börnstein: Numerical Data and Functional Relationships in Science and Technology - New Series
Mass Market
Digest
Trade Paperback
Creep Properties of Heat Resistant Steels and Superalloys, 2004th Edition by K. Yagi - ISBN: 9783540428794
7.60 × 10.63 in
US Letter
mm / in

Returns

This item is eligible for simple returns within 30 days of delivery. Return shipping is the responsibility of the customer. See our returns policy for further details.